New screws and barrels
We supply screws and barrels for all types of injection moulding machines and extrusion lines as well as other special equipment — for plastics processing and the rubber industry alike. The design is chosen according to the machine and the material you process on it.
- Screws — through-hardened, nitrided, PTA-armoured or PVD-coated.
- Barrels — nitrided or bimetallic, with higher resistance to wear and corrosion.
- For specific applications — screws and barrels for compounding and for the rubber industry, including tyre manufacturers.
- Non-return valves and accessories — tip, check ring and seat as a set or individually. Nozzles and heater bands are under spare parts for moulding machines.
Screw and barrel refurbishment
We restore worn screws by hardfacing them with a carbide alloy using PTA (plasma transferred arc) welding. The weld layer does not crack and the working surfaces of the screw last longer — which makes it particularly suitable for filled and abrasive materials. We can also nitride screws and barrels.
| Screw diameter | 35–300 mm |
|---|---|
| Length | up to 8,000 mm |
| Hardfacing hardness | up to 64 HRC |
| Typical lead time | screw refurbishment 1–2 weeks, complete screw and barrel set including nitriding 3–4 weeks |
How to recognise a worn plasticising unit
Wear builds up gradually, so it often shows only in the quality of the parts. Typical symptoms include:
- dosing time increases at the same screw speed,
- the melt cushion and part weight fluctuate,
- black specks, streaks or traces of degraded material appear,
- purging during colour or material changes takes longer than before,
- the non-return valve leaks and holding pressure is unstable.
If you notice any of these symptoms, it is worth measuring the clearance between the screw and barrel and checking the non-return valve. Send us the measurement results with your enquiry.

Choosing the design for your material
The same machine may need a different screw design depending on what it processes. As a guide:
| Material | Main load | Typical design |
|---|---|---|
| Commodity thermoplastics (PP, PE, PS, ABS) | Standard wear | Nitrided screw and barrel |
| Filled materials (glass fibre, mineral fillers) | Abrasive wear | Bimetallic barrel, screw with hard coating |
| PVC, POM and other corrosive materials | Corrosion | Corrosion-resistant design |
| Engineering plastics with high processing temperatures | Temperature and wear | Depends on the specific material and filler |
The table is for guidance only. The final choice depends on the machine, material and operating conditions.